RMC-12-46 An update on Risk Based Inspection: Bringing Focus On External Corrosion Under Insulation, Stress Corrosion Cracking And Other Damage Mechanisms

Joel Presley Inspection Engineer Huntsman Corporation Port Neches, TX Tim Munsterman Technology Director/ Engineering Lloyd’s Register Houston, TX Ed Mullings Director, Capstone RBMI and APM Sales Lloyd’s Register Houston, TX

Format:
Electronic (digital download/no shipping)

Associate Member, International Member, Petrochemical Member, Refining Member - $0.00

Government, NonMember - $35.00

Description:

In 1998 we presented a paper entitled “Using risk based inspection to focus on corrosion under insulation”. We stated that Risk Based Inspection (RBI) was a relatively new technology being applied in the chemical process industry. RBI provided a systematic process for factoring risk into decisions concerning how, where and when to inspect a process plant. The intent of RBI is to focus inspection resources on critical equipment in ways which will prevent failures, particularly catastrophic ones. Such a tool shows the potential to make chemical plants safer in a cost effective way.

Product Details:

Product ID: RMC-12-46
Publication Year: 2012